Structural / Functional Issue

How to Fix Weak Layer Adhesion / Delamination

Step-by-step fix for weak layer adhesion / delamination on Bambu Lab printers including X1C, H2D, P1S, and A1.

How do I fix weak layer adhesion / delamination?

  1. 1

    Increase nozzle temperature by 10–15°C. Higher temps improve layer-to-layer fusion — this is the single biggest factor in inter-layer bond strength.

    Setting: others.nozzle.nozzleTemp

  2. 2

    Reduce cooling fan speed to 50–70% (or 0% for ABS/ASA/Nylon). Excessive cooling prevents the current layer from bonding to the one below.

    Setting: Cooling fan

  3. 3

    Increase layer height slightly (e.g. 0.2mm to 0.24mm). Thicker layers press into the previous layer with more force, improving adhesion.

    Setting: quality.layerHeight

Pro tip: Select "High Strength" above — it increases walls, infill density, and recommends Gyroid infill for maximum inter-layer bonding.

Related Print Issues

Part Breaking Along Layer LinesPoor Dimensional AccuracyPart Too Flexible / Not Stiff EnoughBed Adhesion Failure / Part DetachingSupport Removal Damage / Scars

Still having issues?

Try our AI-powered troubleshooter — describe your problem in your own words and get personalized fixes.

Open AI Troubleshooter

Browse All Print Issues

Uneven First LayerStringing / OozingVisible Layer LinesElephant Foot (First Layer Bulge)Warping / Curling / LiftingVisible Z-SeamRough / Droopy OverhangsBlobs / Zits on SurfaceGhosting / RingingPart Breaking Along Layer LinesPoor Dimensional AccuracyPart Too Flexible / Not Stiff EnoughBed Adhesion Failure / Part DetachingSupport Removal Damage / ScarsInfill Showing Through WallsHeat Creep / Clogging Mid-PrintThin Walls Breaking / Gaps in Thin FeaturesPart Deforms in Heat / SunSpaghetti / Print Detached Mid-PrintUnder-Extrusion (Sparse Lines / Missing Material)Over-Extrusion (Blobby / Too Much Material)Nozzle Clog (Blocked / No Extrusion)Extruder Clog (Filament Stuck in Gears)Filament Sticking to Nozzle (PETG)Bad Bridging Quality (Sag or Snap)Belt Pattern / VFA (Vertical Fine Artifacts)Gaps / Holes in Top LayerDifferent Gloss / Sheen on Different AreasInterlayer Cracking (ABS/ASA/PC/PA)Model Collapsing / Nozzle Hitting PrintWet / Damp Filament (Popping, Bubbles)Layer Shifting (Layers Offset Mid-Print)AMS Filament Tangled / Spool StuckAMS Filament Ran Out Mid-PrintAMS Cutter Stuck / Failed to CutFilament Pile-Up in Waste ChuteBuild Plate Not Detected / Marker MissingPower Loss / Print Resume After OutageHotend Fan Speed Abnormal / StoppedHoming Failed (X/Y/Z Axis)AMS Filament Change Failed / Purge TimeoutChamber Temperature Too High (PLA/PETG Softening)Print Paused — Door / Cover OpenPrinting CF Material with Wrong NozzleCR Touch / BLTouch Leveling FailureSprite Extruder Clicking / Grinding FilamentX/Y Belt Tension Issues (Loose or Over-tight)Klipper Input Shaper / Pressure Advance TuningThermal Runaway Protection TriggeredBed Leveling Springs Losing TensionCreality Print / Slicer Compatibility IssuesPTFE / Bowden Tube Wear or GapIDEX Dual Extruder Calibration OffsetLuban Connection / WiFi Transfer IssuesModule Switching Problems (3D Print / CNC / Laser)Heated Bed Temperature Uniformity (Large Bed)