Cosmetic Issue

How to Fix Different Gloss / Sheen on Different Areas

Step-by-step fix for different gloss / sheen on different areas on Bambu Lab printers including X1C, H2D, P1S, and A1.

How do I fix different gloss / sheen on different areas?

  1. 1

    Reduce outer wall speed to a consistent value (e.g. 80–100 mm/s) or increase it uniformly to 200 mm/s. Gloss variation is caused by different areas printing at different speeds.

    Setting: speed.layers.outerWall

  2. 2

    Disable "Slow down for overhangs" if gloss consistency matters more than overhang quality.

    Setting: Overhang slowdown

  3. 3

    If using fine layers at high speed and seeing fishscale patterns, increase layer height to 0.16–0.20mm.

    Setting: quality.layerHeight

Pro tip: Select "Good Cosmetics" above — it balances speed settings for consistent surface finish across the entire print.

Related Print Issues

Uneven First LayerStringing / OozingVisible Layer LinesElephant Foot (First Layer Bulge)Warping / Curling / Lifting

Still having issues?

Try our AI-powered troubleshooter — describe your problem in your own words and get personalized fixes.

Open AI Troubleshooter

Browse All Print Issues

Uneven First LayerStringing / OozingVisible Layer LinesElephant Foot (First Layer Bulge)Warping / Curling / LiftingVisible Z-SeamRough / Droopy OverhangsBlobs / Zits on SurfaceGhosting / RingingWeak Layer Adhesion / DelaminationPart Breaking Along Layer LinesPoor Dimensional AccuracyPart Too Flexible / Not Stiff EnoughBed Adhesion Failure / Part DetachingSupport Removal Damage / ScarsInfill Showing Through WallsHeat Creep / Clogging Mid-PrintThin Walls Breaking / Gaps in Thin FeaturesPart Deforms in Heat / SunSpaghetti / Print Detached Mid-PrintUnder-Extrusion (Sparse Lines / Missing Material)Over-Extrusion (Blobby / Too Much Material)Nozzle Clog (Blocked / No Extrusion)Extruder Clog (Filament Stuck in Gears)Filament Sticking to Nozzle (PETG)Bad Bridging Quality (Sag or Snap)Belt Pattern / VFA (Vertical Fine Artifacts)Gaps / Holes in Top LayerInterlayer Cracking (ABS/ASA/PC/PA)Model Collapsing / Nozzle Hitting PrintWet / Damp Filament (Popping, Bubbles)Layer Shifting (Layers Offset Mid-Print)AMS Filament Tangled / Spool StuckAMS Filament Ran Out Mid-PrintAMS Cutter Stuck / Failed to CutFilament Pile-Up in Waste ChuteBuild Plate Not Detected / Marker MissingPower Loss / Print Resume After OutageHotend Fan Speed Abnormal / StoppedHoming Failed (X/Y/Z Axis)AMS Filament Change Failed / Purge TimeoutChamber Temperature Too High (PLA/PETG Softening)Print Paused — Door / Cover OpenPrinting CF Material with Wrong NozzleCR Touch / BLTouch Leveling FailureSprite Extruder Clicking / Grinding FilamentX/Y Belt Tension Issues (Loose or Over-tight)Klipper Input Shaper / Pressure Advance TuningThermal Runaway Protection TriggeredBed Leveling Springs Losing TensionCreality Print / Slicer Compatibility IssuesPTFE / Bowden Tube Wear or GapIDEX Dual Extruder Calibration OffsetLuban Connection / WiFi Transfer IssuesModule Switching Problems (3D Print / CNC / Laser)Heated Bed Temperature Uniformity (Large Bed)